About to go take pics.
Meanwhile, I'll leave you with this...

Comparing DLC to Teflon:

Teflon coefficient of friction: 0.05-0.09
DLC coefficient of friction: 0.01
PVD (physical vapor deposition) coatings run around 0.5.
Multiple videos on YT show people cleaning up a DLC BCG with just a single wipe of a dry paper towel without using any solvent.

DLC has a higher max temperature - 1100°F compared to 750°F for Teflon. (some PVD coatings have around the same Max temp as Teflon, some higher)

Hardness...no comparison.
DLC 3000 Vickers.
Teflon 20-40 Vickers.

Carborundum has a hardness of 3100-3400 Vickers.
__________________
Jim
CBOB0497

"That rifle hanging on the wall of the working class flat or laborer's cottage is the symbol of democracy. It is our job to see that it stays there."
- George Orwell
Reply With Quote
 




All times are GMT -4. The time now is 09:28 PM.


Powered by vBulletin® Version 3.8.6
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.